Quote:
Originally Posted by deuce_454 View Post
very nice.... sounds like alot of good impriovements, just one thing... hot zink plating doesnt stiffen the chassis, its a very very wise choice, especialy here in scandinavia.... but the .05mm zink does not in any significant way add rigidity to the frame...

It really changed that frame and itīs actually about 1 mm for both sides. Hot sinc weakens the metal in fact, but it gives the tension for the chassis. So after + and - things I think it is a good improvement to do and it is qoite cheap way to protect the chassis.

0.05 mm you would get with the electrick plating...

Or this is what I have read and learned about Zinc plating.