Just remember another thing about INVERTER machines -- you use a sharpened tungsten on an inverter machine - not balled! I use 2% Ceriated (Orange ends) for my Aluminum work. So if you're going to compare machines -- don't forget that... it DOES make a difference!

For the Syncrowave machines - you'd still ball the tungsten (Green).