Quote:
Originally Posted by GregWeld View Post
Just remember another thing about INVERTER machines -- you use a sharpened tungsten on an inverter machine - not balled! I use 2% Ceriated (Orange ends) for my Aluminum work. So if you're going to compare machines -- don't forget that... it DOES make a difference!

For the Syncrowave machines - you'd still ball the tungsten (Green).
we use sharpened ends on our tig welding of control arms and chassis's
we use 2% thoriated for most everything, in the lincoln 185 unit we have and miller syncrowave 250