Nothing worse than "sugar" on the backside of a stainless weld... ALWAYS back gas when welding SS... no matter what it is if at all possible. You can make up a variety of back gas attachments - tubes - traps etc. - or just purge it if it's a tube like a header etc. It's best to use a dual flow meter... or you loose control and waste gas...
|