Here are some specs that will help you out.. I used to do a lot of outside process for anodizing aluminum..

If you want anodizing with a gloss look.. Parts will need to be polished before sending out to anodizing..

Anodize per AMS-A-8625, Type II, class 2, black- specify material example- 6061-T6 very important that Anodizing house knows the material

This one will give you the titanium look..

Anodize per AMS-A-8625, Type III, Class I, clear(non dyed)- specify material example- 6061-T6 very important that Anodizing house knows the material


Tumbling all aluminum pcs before sending out to anodize is also very important to the finish..

Note: most anodizing houses charge you lot charge for the process.. So.. if you send out 1 or 5.. it will be charged as a lot..