Quote:
Originally Posted by Gonzo
Here are some specs that will help you out.. I used to do a lot of outside process for anodizing aluminum..
If you want anodizing with a gloss look.. Parts will need to be polished before sending out to anodizing..
Anodize per AMS-A-8625, Type II, class 2, black- specify material example- 6061-T6 very important that Anodizing house knows the material
This one will give you the titanium look..
Anodize per AMS-A-8625, Type III, Class I, clear(non dyed)- specify material example- 6061-T6 very important that Anodizing house knows the material
Tumbling all aluminum pcs before sending out to anodize is also very important to the finish..
Note: most anodizing houses charge you lot charge for the process.. So.. if you send out 1 or 5.. it will be charged as a lot..
|
Sounds like you are very knowlegeable on this subject. Do you have a good anodizer that you use presently and if so could you give me their business name and or info. We might have some business for them. It would be much appreciated. Thank you.