12-07-2012, 12:34 PM
|
 |
Senior Member
|
|
Join Date: Jul 2004
Location: Manteca, CA
Posts: 1,299
Thanks: 2
Thanked 48 Times in 26 Posts
|
|
Found a more local supplier for the DPLV line and used that....
The one thing I noticed different is the DP90 says you can sand/scuff after 7 days and do body work etc.... The DPlV says scuff, shoot another coat and then filler etc after 7 days
|