Thread: Tig 102
View Single Post
  #57  
Old 03-11-2013, 09:45 PM
GregWeld's Avatar
GregWeld GregWeld is offline
Lateral-g Supporting Member
 
Join Date: Jul 2005
Location: Scottsdale, AriDzona
Posts: 20,741
Thanks: 504
Thanked 1,080 Times in 388 Posts
Default

Quote:
Originally Posted by Revved View Post
Funny that you mention this as I've just started having this problem.... and interestingly enough I'm welding faster than I used to. Only thing that I've changed is that with steel I've noticed it puddles better when I'm pushing the weld rather than pulling the weld like I do with aluminum so I thought that might have something to do with it.

I'm using 3/16 red stripe (can't remember if that is ceriated or thoriated) tungsten with 1/16 rod as most of what I'm doing is lighter gauge stuff. I did try 1/8" tungsten when I was experienting with the intercooler tubing but with the .065 aluminum tubing I was melting down the tungsten just trying to puddle the weld.



WTF?!?!?!



TIG WELDING IS ALWAYS A PUSH..... MIG you can push or pull.