Originally Posted by GregWeld View Post
BTW ---- I still think you're a bit focused on the "amps" ----- and when learning --- your natural tendency is to weld real slowly.... building too much heat. When you turn your heat down -- way down -- you can focus more on the hand coordination of moving and dabbing and oh crapping....

EEEEEEEEEEHHHHHHHHHAAAAAAAAA
I've been trying to keep the amps low to reduce heat to the point of not having much puddle to dab into thus sticking the rod at the front of the puddle (oh crap) so I'd add a couple amps to the max range. Incorrect torch angle could come into play, tungsten grind, amp/speed/peddle/dab angle/vision, or, or, or.........