Originally Posted by AMPZberlinetta View Post
Thanks for the input on the different tools you are using! I just ordered a couple a those things to try them out. On the metal it almost looks like you have a sanded finish/ has some tooth to it. Is that from the grinding discs or to you go back and sand the metal smooth an orbital or something? Also while making all the panels, are you using a bead roller to stamp in all those strengthening creases? And i promise ill stop asking questions
No worries, ask away.....
Yep, take the metal to at least 150grit before priming as a minimum, in my opinion. I actually go to 220. Crazy paint guys will say 400....
Yep, beadroller. The Trick Tools ones are amazing.