Quote:
Originally Posted by GregWeld View Post
BTW ---- I still think you're a bit focused on the "amps" ----- and when learning --- your natural tendency is to weld real slowly.... building too much heat. When you turn your heat down -- way down -- you can focus more on the hand coordination of moving and dabbing and oh crapping....

EEEEEEEEEEHHHHHHHHHAAAAAAAAA
I've been trying to keep the amps low to reduce heat to the point of not having much puddle to dab into thus sticking the rod at the front of the puddle (oh crap) so I'd add a couple amps to the max range. Incorrect torch angle could come into play, tungsten grind, amp/speed/peddle/dab angle/vision, or, or, or.........
Reply With Quote
 


Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT -7. The time now is 07:41 PM.


Powered by vBulletin® Version 3.8.11
Copyright ©2000 - 2026, vBulletin Solutions Inc.
Copyright Lateral-g.net