I'm fairly new to TIG so I have run into an issue that might have a simple answer...but I'm stumped and I know there are some great welders here... so here goes. I am building a sheet metal brake for another project I thought I would make out of Aluminium I had laying around. I am attempting to attach the legs I made to the main base. I can't seem to join the two and was hoping someone could explain what is going on.

So here is the backstory The main base is 1/4in 6061 and the "legs" are 1/16in aluminum scrap(so I do not know exactly what it is). I thought if I could focus the arc on the thick metal , heat it knowing I am not going to get fantastic penetration, and just melt the thinner metal into the base I could join the two without blowing out the thinner metal. When I strike the arc the tungsten immediately eats away like it would if you struck it without and gas. I tried two different tungstens and both did the same thing. I cleaned the first time with non-chlorinated brake cleaner. I thought it might be something to do with surface prep so I scrubbed with a wire brush and then wiped it down again but no change. I then ran a bead on a scrap piece of aluminium I practiced on previously to check to see if the welder was malfunctioning and that bead was fine. Here is the list of specs and settings I am using:

Eastwood TIG 200 set to AC
3/32 grey tungsten
100% Argon is set at 20
foot pedal at 140amp
Clearance Effect set at -1 and then +1, no difference
#5 alumina cup
pre flow is .5 sec

Here is a shot of the tungsten that is thrashed. This happened immediately as the arc was struck. At least a few mm were lost as the tungsten just kind of dissolved before my eyes.


Here is the work Piece. On the left I got a little bead happening the first try but the tungsten was trashed and I was just trying to glue the pieces together.. I was forcing it. The right is the last attempt where you see the buildup of filler. As soon as the tungsten went the arc looked like a giant cone and immediately melted the thinner aluminium so I tried to get filler in to plug the hole. Ugly and wrong..I know.


I pulled out a practice piece and ran a bead that you will see circled in red. No settings were changed, same type tungsten but a different one since the original two were beyond use, didn't even adjust the pedal just feathered it. Tungsten was fine.


I have accidentally struck an arc without the gas on before and what happened to the tungsten then was exactly what I saw here but the gas was on. I know it has something to do with the work-piece since the welder was fine on the scrap.

Is this somehow because of the thick base plate I was working with? Also, I am a definite newbie to TIG so any comments on the bead on the scrap is welcome, my travel speed was all over the place I know
Reply With Quote
 


Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT -5. The time now is 07:31 PM.


Powered by vBulletin® Version 3.8.11
Copyright ©2000 - 2024, vBulletin Solutions Inc.
Copyright Lateral-g.net