If its 16ga stainless, you wont need to back purge. Just make sure you use .045" filler and keep the machine at 55 amps. Its all about the heat in the weld. Use 347 stailess filler. You can accomplish this without crystallizing the back side. I do back purge collectors because there is so much heat in that one area.I also use stainless filler for ALL my mild steel headers and exhaust. 309L filler.

Hope this helps.
Reply With Quote
Reply


Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT -7. The time now is 05:14 AM.


Powered by vBulletin® Version 3.8.11
Copyright ©2000 - 2025, vBulletin Solutions Inc.
Copyright Lateral-g.net