Quote:
Originally Posted by Rhino View Post
Solid core wire requires the use of a shielding gas which is external to the filler material. The flux core wire burns the flux creating the shielding gas cloud. For this to happen the gas has to travel through the molten puddle causing a less attractive, and potentially more porous, weld. For anything that's going to be cosmetic (such as body panels) you'll want to use the gas. You can get by without using it, but it will make things much easier.
Basically -- FLUX CORE wire is for farmers in the field - not nice cars....

ROFLMAO... sorry - but it's true.
Reply With Quote
 


Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT -7. The time now is 09:58 PM.


Powered by vBulletin® Version 3.8.11
Copyright ©2000 - 2026, vBulletin Solutions Inc.
Copyright Lateral-g.net